Cold Shrink Tube Silicone Rubber for Weather Proof


Cold Shrink Tube, also is known well as “Cold Shrink Wrap”, is manufactured with silicone rubber for weatherproofing protection on telecommunication equipment connections, such as RRU, Antenna and Microwave. Comparing with tape sealing protection, cold shrink tube installation is much shorter (15-30 seconds), convenient installation, uniform appearance for acceptance.

Recursos

» Easy and quick installation

»Não requer ferramentas ou calor

»Oferece boa estabilidade térmica

»Acomoda uma ampla variedade de tamanhos de cabos

»Excelente resistência ao rasgo

» UV and ozone aging resistant

Note: In certain applications, a foam tape will be needed for smaller cable diameter that cannot be covered with the tube range, the foam tape is used to increase the smaller cable diameter and assure the sealing of clod shrink tube.

Properties

ItemParameter and ResultTest Method
À prova d'águaClassPass, IPX7IEC 60529:1989/AMD2:2013/COR1:2019

1 meter depth in water, duration: 30 minutes

Physical and mechanical propertiesShore HardnessA/41/1ASTM D2240-15
Resistência à tração9.66 MPaASTM D412-16 Method A
Elongation930%ASTM D412-16 Method A
Força de rasgo28.4 N/mmASTM D624-00
Brittleness Temperature by ImpactPassarASTM D746-14,-60℃
Drop TestPassar

No damage, deformation, and support tube could be pulled out normally

Drop from height 1.2m on tile floor surface, 3 times to test
FlammabilityHorizontal BurningHBUL 94-2013 Rev.14-2022 Section 7
ElectricityRigidez dielétrica19.10 KV/mmASTM D149-20 Method A
Performance under harsh environmentMechanical and Waterproof PropertiesNo crack, discoloration, damage or deformation,

IPX7 Pass

 

1. Dry heat test (IEC 60068-2-2:2008 Test Bb): 90±2℃,168 hours;

2. Low temperature test (IEC 60068-2-1:2008Test Ab): -40±2℃,168 hours;

3. Thermal cycling test: Cycle time:12h/cycle, Cycle index: 10 cycles, Total duration: 120 hours;

4. Damp heat test, cyclic test (IEC 60068-2-30:2005 Test Db):Cycle time:24h/cycle, Cycle index: 10 cycles, Total duration: 240 hours;

5. Damp heat test, steady state (IEC 60068-2-78:2012 Test Cab):Temperature: 75±2℃, Humidity:(95±1) %RH, Total duration: 1000 hours

Aging TestLight Aging Test-UV ExposureNo crack, discoloration, damage or deformation

Grey scale: 4-5

IPX7 Pass

ISO 4892-3:2016Cycle1& ISO 105-A02:1993/Cor.2:2005

Lamp type: UVA-340, 8h UV at (60±3)℃ BPT,0.76W/(m²×nm)@340nm

4h condensation at(50±3)℃ BPT

Exposure duration:1000 hours

Ozone AgingNo crack, discoloration, damage or deformation,

IPX7 Pass

ASTM D1149-16 Method B procedure B1

Temperature: 40±1℃

Ozone concentration:50±5 pphm

Exposure duration: 72 hours

Hailstone Resistant TestNo crack,damage or deformationIEC 61215,φ20mm hailstone falling
MaterialEnvironmental ProtectionRoHS

Reach

IEC 62321

SVHC

TemperaturaInstallation Temperature-40℃ ∼ 60℃Refer to “mechanical properties” and “performance under harsh environment”
Operation Temperature-60℃ ∼ 80℃
Stock Temperature-60℃ ∼ 80℃

How to Install a Cold Shrink Tube